A process combination of ion exchange and electrodialysis for the recovery and purification of hydroxy acids from secondary sources

Heinonen, Jari; Zhao, Yan; Van der Bruggen, Bart (2020-01-30)

Katso/Avaa
heinonen_et_al_a_process_finaldraft.pdf (5.863Mb)
Lataukset: 


Post-print / Final draft

Heinonen, Jari
Zhao, Yan
Van der Bruggen, Bart
30.01.2020

Separation and Purification Technology

Elsevier

School of Engineeering Science

https://doi.org/10.1016/j.seppur.2020.116642
Näytä kaikki kuvailutiedot
Julkaisun pysyvä osoite on
https://urn.fi/URN:NBN:fi-fe202002034279

Tiivistelmä

Ion exchange and electrodialysis processes for the production of hydroxy acids (HAs) from alkaline soda and kraft black liquors (BLs) were investigated. Ion exchange with a type-2 strong anion exchange resin in sulfate form was used to separate thiosulfate from alkaline kraft-BL-based mixture of Na+ salts of HAs. Efficient regeneration of the spent resin to sulfate form was achieved only through hydroxide form. Ion exchange with strong cation exchange (SAC) resins was successfully used to convert the Na+ salts of HAs in soda-BL-based solution and thiosulfate-free kraft-BL-based solution into free acids with complete removal of Na+ ions from the solution. The spent resin was efficiently regenerated with 1–2 mol/L H2SO4. Electrodialysis with bipolar membranes (EDBM) was used for the generation of H2SO4 and NaOH from the spent SAC resin regenerants (Na2SO4–H2SO4 mixtures). Overall, 1 mol/L H2SO4 with 95% purity and 90% yield could be obtained, but excess water flux through the membranes limited the maximum obtainable H2SO4 concentration to 1.17 mol/L. Simultaneously, 0.79 mol/L NaOH was produced with 93% purity. EDBM-based H2SO4 was successfully used for the regeneration of the SAC resin. With EDBM, a closed loop can be built for the regeneration of SAC resin with the simultaneous generation of NaOH. The results of this study demonstrate that a process combination of ion exchange and electrodialysis decreases the overall chemical consumption related to HA production and enables efficient chemical recycling.

Lähdeviite

Heinonen, J., Zhao, Y., Van der Bruggen, B. (2020). A process combination of ion exchange and electrodialysis for the recovery and purification of hydroxy acids from secondary sources. Separation and Purification Technology. DOI: 10.1016/j.seppur.2020.116642

Kokoelmat
  • Tieteelliset julkaisut [1136]
LUT-yliopisto
PL 20
53851 Lappeenranta
Ota yhteyttä | Tietosuoja | Saavutettavuusseloste
 

 

Tämä kokoelma

JulkaisuajatTekijätNimekkeetKoulutusohjelmaAvainsanatSyöttöajatYhteisöt ja kokoelmat

Omat tiedot

Kirjaudu sisäänRekisteröidy
LUT-yliopisto
PL 20
53851 Lappeenranta
Ota yhteyttä | Tietosuoja | Saavutettavuusseloste