From waste to high-performance insulators : tailoring polyimide aerogels from polyurethane recycling streams

Nguyen, Hoang Nhung (2026)

Katso/Avaa
Mastersthesis_Nguyen_Hoang Nhung.pdf (4.786Mb)
Lataukset: 


Diplomityö

Nguyen, Hoang Nhung
2026

School of Engineering Science, Kemiantekniikka

Kaikki oikeudet pidätetään.
Näytä kaikki kuvailutiedot
Julkaisun pysyvä osoite on
https://urn.fi/URN:NBN:fi-fe20260827120345

Tiivistelmä

Polyimide aerogels (PIAs) are attractive for their low density, thermal stability, fire resistance, and low thermal conductivity. However, their conventional production relies on hazardous solvents and fossil-derived monomers. This study investigates a more sustainable approach for PIA production by reducing hazardous N-methyl-2-pyrrolidone (NMP) usage, optimizing poly(amic acid) (PAA) solid loading, and exploring the recovery of 4,4′-methylenedianiline (MDA) from polyurethane waste as a potential renewable monomer source. BPDA-MDA-based PIAs were prepared following the conventional two-step route, including PAA synthesis, freeze-drying, and thermal imidization. Among six solvent systems investigated, a mixture of NMP and A/B blend (formulation II or SF-II) provided the best overall balance between solvent substitution and aerogel performance, enabling substantial replacement of NMP while maintaining a bulk density of 0.100 ± 0.004 g cm⁻³, a low thermal conductivity of approximately 0.020 W m⁻¹ K⁻¹, a glass transition temperature of 254 °C, and a 5% mass-loss temperature (Td5%) of 539 °C. The resulting aerogels exhibited coherent porous morphologies, good dimensional stability, hydrophobic surfaces, and thermal-insulation performance comparable to that of the NMP-derived reference. Using this solvent system, the influence of PAA solid loading (3–10 wt.%) was investigated. Increasing solid loading increased bulk density from 0.05 to 0.13 g cm⁻³ and compressive modulus from 0.14 to 2.88 MPa, while thermal conductivity increased from 0.015 to 0.023 W m⁻¹ K⁻¹. In contrast, thermal stability remained essentially unchanged, with Td5% values of 539–542 °C and char yields of 56–58 wt.%. Based on the combined structural, thermal, and mechanical results, the 7 wt.% formulation provided the most balanced overall performance. An exploratory polyurethane glycolysis-hydrolysis route indicated the formation of MDA-containing fractions, but further purification was required before incorporation into polyimide synthesis. Overall, this work demonstrates the feasibility of a reduced-NMP route for PIA production and establishes a foundation for future integration of waste-derived MDA into a more circular manufacturing process.
Kokoelmat
  • Diplomityöt ja Pro gradu -tutkielmat [15768]
LUT-yliopisto
PL 20
53851 Lappeenranta
Ota yhteyttä | Tietosuoja | Saavutettavuusseloste
 

 

Tämä kokoelma

JulkaisuajatTekijätNimekkeetKoulutusohjelmaAvainsanatSyöttöajatYhteisöt ja kokoelmat

Omat tiedot

Kirjaudu sisäänRekisteröidy
LUT-yliopisto
PL 20
53851 Lappeenranta
Ota yhteyttä | Tietosuoja | Saavutettavuusseloste